Renewable Energy

Emulsion buffer layer curbs screen-printing degradation in copper-plated HJT solar cells

Chinese researchers traced efficiency loss to worn screen mesh knuckles and found a 4.7% emulsion coverage ratio best balances wafer protection against photoresist uniformity.

Signe HalvorsenNovember 15, 20265 min read0 views

A conceptual printing screen with a patterned emulsion buffer layer hovering above a copper-gridded silicon wafer in a clean production setting.

Researchers in China have traced the mechanism by which repeated screen printing degrades copper-plated silicon heterojunction (HJT) solar cells and have proposed a modified screen design intended to limit the damage. The findings were published in Solar Energy.

Screen printing is a workhorse of solar cell metallization, but the mechanical pressure and thermal treatment involved can harm the sensitive passivating contact structures of HJT devices, raising recombination losses and pulling down conversion efficiency. That matters more for copper-plated HJT cells, which are seen as a route to lower metallization costs and reduced dependence on silver.

Why photoresist printing differs from silver paste

Corresponding author Lang Zhou told pv magazine that photoresist printing in HJT production differs fundamentally from conventional silver paste printing. In silver paste screens, openings cover only 2–5% of the total area and the remaining surface carries an emulsion layer that keeps the mesh from touching the wafer. Full-area photoresist coating, by contrast, typically uses a screen without emulsion coverage so that resist is deposited evenly across the whole wafer, meaning the mesh comes into direct and extensive contact with the wafer on every printing cycle.

Earlier production investigations cited by the team showed conversion efficiency slipping from 26.2% to 25.7% across 15,000 consecutive printing cycles. Open-circuit voltage and fill factor accounted for most of the loss, while short-circuit current density and electrical resistance stayed largely unchanged. Minority carrier lifetime degradation rose from 0.61% with a new screen to 11.0% after 15,000 cycles.

Knuckle wear and a 4.7% emulsion buffer

Using three-dimensional confocal microscopy, the scientists linked the decline to progressive wear of the screen mesh knuckles. As knuckles flatten, their contact area with the wafer grows and mechanical stress on the passivation layers underneath increases. Scanning electron microscopy showed no visible surface scratches, but photoluminescence measurements recorded higher recombination losses, pointing to damage at the amorphous silicon/crystalline silicon interface.

To break the direct contact, the team added an emulsion buffer layer to the screen and tested six patterns with emulsion coverage ratios between 2.9% and 16.6%. The trials revealed a trade-off: greater coverage protected the wafer but disturbed photoresist distribution. A coverage ratio of 4.7% gave the best balance, holding minority carrier lifetime degradation to 0.41% after 10,000 cycles while keeping coating uniformity reasonably good.

Zhou said the results show that a relatively simple change to screen design can substantially mitigate printing-induced degradation, offering a practical way to improve manufacturing reliability for copper-plated HJT cells.

Copper metallization momentum

The study arrives as copper draws growing interest as a substitute for silver contacts in HJT cells. In April 2026, researchers at China's Nankai University reported a silver-free HJT cell at 25.2% efficiency, combining plasma-induced interface engineering with copper electroplating to tackle adhesion, contact resistance and stability at the ITO interface. Separately, scientists at Germany's Forschungszentrum Jülich reached 23.08% with a fully copper-metallized HJT device, a relatively small penalty versus its silver counterpart, while a version using silver-copper paste on the front and silver contacts on the rear hit 23.95%.